Introduce the S-TEN1 S-TEN2 (Sulfuric Acid and Hdrochloric Acid Dew-Point Correcsion-resistnat steel) S-TEN 系列鋼材介紹
Good day !
Today we want to introduce the series of S-TEN®.
今天來跟大家介紹S-TEN 系列鋼材
As the original products of NIPPON STEEL AND SUMITOMO METAL.
The Sulfuric Acid and Hdrochloric Acid Dew-Point Correcsion-resistnat steel is mainly used in follwoing case.
The flue-gas treatment facility (such as chimney) of coal-fired boilers and waste incineration plants, etc.
Hydrochloric Acid pick-ling, Hydrochloric Acid and other tanks.
耐硫酸・鹽酸露點腐蝕鋼板是屬於新日鐵住金的原創商品, 大多使用在:
石炭火力鍋爐或者是廢棄物燃燒設施等等排煙設備
鹽酸洗槽和工業硫酸槽等等的材料
Merit of the S-TEN
With similar strength, workability, weldability compare to the general steel
More economical than stainless steel
With a rich product line rang from hot -rolled sheets (plates), cold -rolled sheets and pipe and tubes to welding materials.
S-TEN 鋼材的優點
等同於一般鋼材的韌度、延展性以及熔接性
相較於不銹鋼的更具經濟性
冷軋鋼板、熱軋鋼板、鋼管、熔接材料等等多種類的型態
There are two standards of S-TEN. Both of them with the advantages of the sulfuric acid and hydrochloric acid resistant characteristic.
The expression of JIS standard as following :
S-TEN1 ⇒ JIS G 3106 appropriate for SM400
S-TEN2 ⇒ JIS G 3106 appropriate for SM490A
Therefore, the tensile strength of S-TEN2 will be equivalent to 50kgs of steel.
S-TEN系列材質有兩種規格。兩種都具有耐腐蝕的特性,以JIS規格來表示則如下圖所示
S-TEN1 ⇒ JIS G 3106 適用於 SM400
S-TEN2 ⇒ JIS G 3106 適用於SM490A
因此,S-TEN2的抗拉强度相當於50KG的一般鋼材
In Kumagai , we will recommend to classify the S-TEN1 and S-TEN2 according to use environment.
S-TEN1 ⇒ use for normal temperature (under 300℃)
S-TEN2 ⇒ use for high-temperature (300℃~500℃)
在熊谷特殊鋼,我們推薦以使用環境來分類S-TEN1以及S-TEN2
S-TEN1 ⇒ 適合於一般溫度下 (300℃以下)
S-TEN2 ⇒適合高溫環境(300℃~500℃)
Although the S-TEN1 with the sulfuric acid and hydrochloric acid resistant characteristic, but it will become fragile in the high-temperature environment. Therefore we will recommend the S-TEN2 for using in high-temperature environment such as flue-gas treatment facility.
In Kumagai , we can not only provide the detail information of the S-TEN1 , S-TEN2 but also the processing service for bending or different sizes of cutting.
ABREX®・WEL-TEN®・S-TEN® is the trademark of NIPPON STEEL CORPORATION
COR-TEN®is the trademark of United States Steel Corp.
ABREX®・WEL-TEN®・S-TEN® 是屬於日本制铁(株)的登錄商標
COR-TEN®是屬於United States Steel Corp.的登錄商標